Operation CHARM: Car repair manuals for everyone.

Aluminum Alloy Repair

Safety Precautions

Precautions for Ensuring Safety:

1. Although aluminum is non-toxic, it is lightweight, so fine particles of metal given off by sanding operations tend to float in the air. It is therefore vital that operators protect their lungs and eyes from this dust.
2. Small pieces of aluminum alloy are spattered by MIG welding can be projected over considerable distance. It is therefore important to provide protection not only for the welders operators themselves, but also for anyone in the surrounding areas.
3. The sparks generated from the arc during inert gas are welding are very bright and may hurt the eyes if viewed directly. A protective shield for the eyes must therefore be worn at all times when welding.

Use of protective gear to ensure safety:
Work overalls with long sleeves, a cap, and safety shoes must be worn at all times. Depending on the job to be done, protective goggles, gloves, ear plugs, and a dust-proof mask should also be worn.

CAUTION:
- When aluminum alloys are heated, they melt without changing color.

Melting temperature

Aluminum alloys: Approx. 1184 degrees F (640 degrees C) (depends on alloy)

Steel plate: Approx. 2732 degees F(1500 degrees C)

- Aluminum alloys can be repaired in virtually the same way as steel sheets, but it is important to have a good grasp of their properties and be thoroughly familiar with their limitations.

- Aluminum alloys tend to overheat during sanding. When they overheat, the metal tends to flake and clog the filing surface of the sanding tool. If a tool with a clogged surface is used, it will leave scratches and marks on the base metal.