Operation CHARM: Car repair manuals for everyone.

Welding Precautions




Welding Precautions


Material:






NOTE: Whenever factory E-coat has been removed by sanding, grinding or weld burn-off, the coating must be restored. Use low temperature anti-corrosion coating.

1. If welding must be done on a frame, make sure the following requirements are met:
- If the frame is attached to the vehicle, the battery ground cable must be disconnected before using any electrical welding equipment.
- Do not use gas welding equipment.
- Use a temperature-indicating crayon to make sure that the temperature does not exceed 750°C (1,400°F).
- Install new welded components by heliarc, stick or MIG welding where possible. If heliarc, stick or MIG welding is not possible, use puddle welding.