Undamaged Window Glass, Preparing for Glazing
Undamaged Window Glass, Preparing for Glazing
Adhesive Bead, Cutting
Do not prime the adhesive surface or use a cleaning solution on it. Keep the adhesive surface free of dirt and grease.
Do not yet treat the cut adhesive surface with the activator.
• When re-using an undamaged window, cut back remaining adhesive sealant to 1 to 2 mm shortly before re-adhering, do not damage primer and ceramic coating.
• Residual material acts as a base for the new adhesive sealing material.
Exception: If the bonding is going to be performed longer than one day after cutting back the adhesive bead, then then remaining material must be activated with the activator.
Apply the activator evenly and in one wiping motion using the applicator.
Do not let the activator come in contact with the paint because this will damage the paint.
Drying time is approximately 10 minutes.
Exception: if the window is not bonded immediately after cutting back the adhesive, the remaining material must be activated with the activator (D 181 801 A1).